Process of T10 Manufacture



                --The flow chart of custom rims



                                                   RAW             Strictly control material quality.                                                      FINISHING
                                               MATERIAL            Material formula specifically
                                                                   adjusted for rims.
                                                                                                                                                     anodizing, powder coating...



                                                                   Preheat small column for about
                                              EXTRUSION            4-5  hours,  extrude  through                                                      EXTRA WORKINGS
                                                                   molds  make  long  aluminum
                                                                   stick.
                                                                                                                                                 CNC machining, side brush, safety
                                                                                                                                                 indicator, eyelets,
                                                                   Round aluminum stick into 3 or                                                decal install...
                                              ROUNDING             2 combine pieces of rim then

                                                                   cut into individual rims.



                                                                   Pin & sleeve joint, firstly press
                                                                   one side to fix the pins. Joint
                                               JOINTING            the rim then press the other
                                                                   side to make sure the rim joint                                                   FINISHED PRODUCT
                                                                   steadily.



                                           COLD WORKING            Specific mold and roller wheels.
                                                (FORMING)          Roll each rim two times.





                                              ARTIFICIAL           In 180℃ for 8 hours. Cool off
                                                 AGING             with big fans.
                                            (HEAT TREATMENT)                                                                                                            PACKING





                                                  HOLE             Standard/ Custom
                                              PUNCHING/            Avarage, paired, triple cluster,
                                               DRILLING            angle/ size of spoke hole.